MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Aperam Superimphy® 22 Bar-Corrosion application
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: SY22 is a fully austenitic advanced corrosion resistance alloy that offers resistance to both aqueous corrosion and attack at elevated temperatures but also good tensile properties.

Applications:

  • Chemical industries (sulfuric acid, hydrochloric acids, nitric acids, ferric and cupric salts,…)
  • Petrochemical processing
  • Pollution control (Flue gas desulfurization)
  • Pulp and paper industry
  • Marine applications
Standards related to these applications: ASTM B574 and B564, NACE MR0175

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 20 - 22.5 %
Cobalt, Co <= 2.5 %
Iron, Fe 2.0 - 6.0 %
Molybdenum, Mo 12.5 - 14.5 %
Nickel, Ni 51 - 63 %
Tungsten, W 2.5 - 3.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications
Haynes 214® Alloy Sheet
ATI Allvac® Nickelvac® C-276 UNS N10276 Nickel Superalloy
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel

NPERA018 / 194807

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.