MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Durethan® B 35 FKA 000000 Nylon 6 (PA6), Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: PA 6 Film grade, medium viscosity, nucleated, with processing and slip additives, in compliance with FDA for food contact

Application Examples: flat and blown film, flat film coextrusion for PA/PE composite films

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Moisture Absorption at Equilibrium 3.0 %50% RH; ISO 62
Water Absorption at Saturation 10 %ISO 62
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 40.0 MPaISO 2093-1
Tensile Strength, Yield 35.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 25 %50 mm/min; ISO 527-1,-2
Tensile Modulus 800 MPa1 mm/min; ISO 527-1,-2
Flexural Yield Strength 20.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 700 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 8.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 7.50 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 5.00 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 60250
 18
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding
Mold Temperature 40.0 °Cinjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 388 Aramid Fabric
Hexcel® HexForce™ 1629 Aramid Fabric
Envalior Durethan® T 40 ZS 000000 Partially aromatic polyamide
Envalior Durethan® T 40 000000 Partially aromatic polyamide
Envalior Durethan® BKV 50 H2.0 EF 900116 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned

PLANW9273 / 208074

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.