MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
CEN® Electronic Material BL Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CEN®BL polyimide film is a printable film that has the same thermal and chemical properties as CEN®CN Polyimide Film, which offers excellent performance in temperatures from -269-400°C. CEN®BL is pigmented to provide contrast and eliminate the need for opaque coatings. Printing on BL can be accomplished with thermal transfer and laser printing.

Applications: Labels for high temperature, cryogenic storage, harsh chemical environments, and printed circuit board identification.

All information provided by CEN Electronic Material Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/cc
Thickness 46.0 - 54.0 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 145 MPaASTM D882
Film Tensile Strength at Yield, TD 135 MPaASTM D882
Elongation at Yield >= 45 %ASTM D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Surface Resistivity per Square >= 1.00e+13 ohmASTM D257

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CEN® Electronic Material BX Polyimide Film
CEN® Electronic Material HT Polyimide Film
CEN® Electronic Material CS Polyimide Tape
CEN® Electronic Material CF 120CF616 Polyimide Film
CEN® Electronic Material CN Polyimide Film, 1 Mil Thickness

PCENE004 / 93466

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.