MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Fiber: T1000 12K 5H Satin, 283 g/m2

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccNominal Laminate Density
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1425 MPa
@Temperature 23.0 °C
prEN2561 Type B
Tensile Modulus 89.0 GPa
@Temperature 23.0 °C
prEN2561 Type B
Compressive Yield Strength 925 MPa
@Temperature 23.0 °C
prEN2580 Type A
Shear Modulus 4.70 GPa
@Temperature 23.0 °C
In-Plane; prEN6032
Shear Strength 43.0 MPa
@Temperature 140 °C
ILSS; prEN2563
 50.0 MPa
@Temperature 80.0 °C
ILSS; prEN2563
 51.0 MPa
@Temperature 23.0 °C
ILSS; prEN2563
 52.0 MPa
@Temperature 100 °C
ILSS; prEN2563
 54.0 MPa
@Temperature 120 °C
ILSS; prEN2563
 118 MPa
@Temperature 23.0 °C
In-Plane; prEN6032
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Cured Thickness per Ply (cm)0.0308
Fiber Volume (%)51

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RSP Technology RSA-441 T6 Aluminum Super Alloy
RSP Technology RSA-444 T6 Aluminum Super Alloy
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape Not Supported 150 g/m2
Hexcel® HexPly® 920KX-285-52% 125°C Curing Epoxy Matrix

PHEXC175 / 98646

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.