Product Description: 50 Shore D TPE/TPO hybrid for injection molding applications. This grade offers flexibility, good resilience, and compatibility with Polypropylene. Availability: North America Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Processability; High Elasticity; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Resilient; Solvent Resistant; UV Resistant Processing Method: Extrusion; Injection Molding Information provided by Entec Polymers |