MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller HydroArmor® 7740 Fire Retardant Protective Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: A sprayable, latex product designed for use on steel, aluminum, fiberglass, and plywood. This highly fire resistant material can be easily sprayed onto overhead and vertical surfaces to seal joints. Heavy wet film builds can be applied without runs, drips or sagging to bridge seams. Because this material is filled with hollow microspheres, this coating adds little weight to vehicle bodies, even at high film builds. Our lab test of HydroArmor®7740 show that it is extremely durable under even the worst service conditions; several days at 96°C (205°F) and immersion in acidic and caustic solutions did not affect dried beads of this material. Beads did not lose adhesion or crack when test panels were bent at 34°C (-30°F). After weeks of exterior exposure cycling, the HydroArmor® coating remained intact and there was no adhesion loss. The highly flammability resistance and low smoke generation results obtained when tested under ASTM E162 and E662 permit this product to be used on passenger rail cars. HydroArmor®7740 dries quickly at ambient temperatures or can be force dried after only 30 minutes dry time at room temperature. HydroArmor® 7740 is as safe to use and as easy to clean up as latex house paint. HydroArmor® 7740 provides better protection than any of the competitive products we’ve tested without environmental and safety problems inherent in many of the undercoatings available today.

Application: As with any adhesive or sealant, all loose dirt and dust should be removed from the surface to be coated before application. HydroArmor®7740 is designed to be applied with airless spray equipment. With this equipment, we can spray at 50 to 60 pounds air pressure using spray tips with orifices from .019” to .035”. As with all air motor pumps, adequate air volume is required. HydroArmor® resists water washoff after air drying 30 minutes at 45 - 55% relative humidity; if not baked, it dries through in 24 hours or less (drying is slowed by high humidity and poor air circulation). Until HydroArmor ®7740 dries, overspray can be removed and equipment can be cleaned with water. Dried material can be removed with Methyl Ethyl Ketone.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.710 - 0.770 g/cc
Solids Content 45 - 48 %
Volatile Organic Compounds (VOC) Content 13 - 15 g/l
pH 9.0 - 10
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL132 / 316923

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.