System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Sumitomo Bakelite E 8398 Epoxy Molding Compound
Categories:
Polymer
;
Thermoset
;
Epoxy
;
Epoxy Molding Compound
Material Notes:
E 8398 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.83
g/cc
ASTM D792
Apparent Bulk Density
0.900
g/cc
Powder; ASTM D1895
Water Absorption
0.20 %
@Time 173000 sec
ASTM D570
Linear Mold Shrinkage
0.0050
cm/cm
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength
76.0
MPa
ASTM D638
Flexural Strength
159
MPa
ASTM D790
Flexural Modulus
17.0
GPa
ASTM D790
Compressive Strength
276
MPa
ASTM D695
Izod Impact, Notched
19.0
J/m
ASTM D256A
Electrical Properties
Original Value
Comments
Dielectric Constant
3.9
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength
>=
15.4
kV/mm
@Frequency 60 Hz
SS, dry
>=
16.1
kV/mm
@Frequency 60 Hz
SS, wet
>=
21.1
kV/mm
@Frequency 60 Hz
ST, dry
>=
22.0
kV/mm
@Frequency 60 Hz
ST, wet
Dissipation Factor
0.014
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance
180
sec
ASTM D495
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
19.0
µm/m-°C
ASTM E831
CTE, linear, Transverse to Flow
28.0
µm/m-°C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi)
215
°C
As Molded; ASTM D648A
>=
282
°C
Post Baked; ASTM D648A
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Emerald Performance Materials EPALLOY® 8330 A85 Epoxy Phenol Novolac Solution
Elantas EN-8 (Conap) Casting, Potting, and Molding Compound
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade
PSUMIT136 / 193941
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.