MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Domo TECHNYL® 1021ST PA6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Description: Polyamide 6, unfilled, super tough impact modified, for injection molding

Available in: Asia Pacific

Product Applications: TECHNYL® 102ST has the highest level impact strength and balanced mechanical properties. It is suitable for all sectors industries such as: Bowling pin, Brake drum, Inline skate part. This product is available natural colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Constant 4.0IEC60250
Dielectric Strength 18.0 kV/mmIEC 60243
Dissipation Factor 0.12IEC 60250
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
Domo Technyl® A218 Heat Stabilized Nylon 66
Covestro Texin® STX Thermoplastic Polyurethanes (TPU)
Covestro Desmopan® 9885DU TPU

PRHOD567 / 137798

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.