MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Ceramics ALC Alumina Insulation
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 g/cc
Open Porosity 93 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 100 psi
@Strain 60 %
Load applied normal to fiber plane, strain = load deformation in mils; Three Point Bending, sample 0.5"*0.5"*4"
 100 psi
@Strain 40 %
Load applied parallel to fiber plane, strain = load deformation in mils; Three Point Bending, sample 0.5"*0.5"*4"
Compressive Yield Strength 10.0 psi
@Strain 8.0 %
Load applied normal to fiber plane
 12.0 psi
@Strain 4 %
Load applied normal to fiber plane
 30.0 psi
@Strain 4 %
Load applied parallel to fiber plane
 50.0 psi
@Strain 8.0 %
Load applied parallel to fiber plane
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.250 BTU/lb-°F
Thermal Conductivity 0.0700 W/m-K
@Temperature 400 °C
parallel to thickness; ASTM C177-76
 0.130 W/m-K
@Temperature 800 °C
Parallel to Thickness; ASTM C177-76
 0.190 W/m-K
@Temperature 1100 °C
Parallel to Thickness; ASTM C177-76
 0.260 W/m-K
@Temperature 1400 °C
Parallel to Thickness; ASTM C177-76
 0.280 W/m-K
@Temperature 1650 °C
Parallel to Thickness; ASTM C177-76
Melting Point 1870 °C
Maximum Service Temperature, Air 1550 °CContinuous
 1650 °CIntermittent
Shrinkage 1.0 %
@Temperature 1550 °C,
Time 3600 sec
Perpendicular to Thickness
 3.0 %
@Temperature 1650 °C,
Time 3600 sec
Perpendicular to Thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 85 %
SiO2 15 %
 
Descriptive Properties
BondSilica
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CZIR053 / 2861

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.