MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SCG Chemicals H568JA High density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: SCG HDPE H568JA is a high density polyethylene resin with excellent environment stress cracking resistance and good mechanical properties balance. It is particularly designed for light-weight carbonated soft drink caps. This resin have excellent process ability for both injection and continuous compression molding. Related Finished Products: Caps and closures for carbonated soft drinks and hot fill beverages.

Applications: Beverage caps and closures (carbonated soft drink, sparkling water).

Features: Excellent process ability. Excellent environmental stress cracking resistance. Good mechanical property. Good organoleptic property.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.956 g/ccASTM D 1505
ESCR 10% Igepal® >= 600 hourF50, condition B, compression molded; ASTM D1693
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ASTM D2240
Tensile Strength at Break 14.0 MPa1B, speed 50 mm/min; ISO 527
Elongation at Yield 7.0 %1B, speed 50 mm/min; ISO 527
Tensile Modulus 1100 MPa1B, speed 1mm/min; ISO 527
Izod Impact, Notched 49.0 J/mISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CASTM D648
Vicat Softening Point 123 °CASTM D1525
 
Descriptive Properties
AppearanceBlock pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC719 / 277976

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.