MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 9392 Flexible Potting Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 9392 is a low viscosity, two-part polyurethane formulation recommended for potting and molding where flexibility and temperature resistance are required. TRA-BOND 9349 is a room temperature-curing system that bonds to metals, plastics, glass, and ceramics, and is an electrical insulator with good thermal and impact resistance.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccMixed
Viscosity 17000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Tensile Strength, Yield 1000 psi
Adhesive Bond Strength 600 psiLap shear, adhesion to glass
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
Dielectric Constant 4.3
@Frequency 1e+6 Hz
 7.0
@Frequency 1000 Hz
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hour
@Temperature 82.0 °C
 168 hour
@Temperature 24.0 °C
 
Descriptive Properties
Color Clear, Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Hexcel® Redux® 312 Modified epoxy film adhesive (0.015 psf)
Henkel Hysol EA 9321 Paste Adhesive System

PTRAC209 / 71137

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.