MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide
Categories: Metal

Material Notes: Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut Gaskets

Available Forms: Die-Cut Elastomer with Joined EMI Strips.

Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 20 - 30 dB
@Frequency 14000 Hz
 83 - 93 dB
@Frequency 1e+9 Hz
 >= 102 dB
@Frequency 1.80e+7 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 66.0 °CNeoprene Version
 204 °CSilicone Version
Minimum Service Temperature, Air -62.0 °CSilicone Version
 -34.0 °CNeoprene Version
 
Descriptive Properties
Maximum Joint Unevenness, % of Gasket Height0.25Class C- Completely Interchangeable
 0.3Class A- Permanently Closed
 0.3Class B- Open-Close in Same Position

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 K8 9 FR grey (3840) PA6 FR, Dry, 20% Glass Filled
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets
Saint-Gobain Chemfab® TCK® 1000 High-Strength Leno Weave Open Mesh Belting Material
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6
PTS Trimid® N6-200L Nylon 6 with Lube

PCHOME293 / 131003

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.