Key features: Vacuum Molding. Common Uses: Stirred type yogurt container.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and heat-resistance. Data provided by Korea Kumho Petrochemical Co., Ltd. |