Features and Typical Applications Ability to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in harsh environments. Typical applications include sensors, transformers, power supplies, and rectifiers.
Emerson & Cuming 5954 Stycast® Two-Component Silicone High Service Temp Encapsulant
- Thermally Conductive
- Poor Chemical Resistance
- Filled
- Mix Ratio by Weight = 100:100
Cure Type: Room Temp or Heat Bonding Type: Silicone The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |