Hostacom G3 U01 102297 is a 30% glass fiber reinforced PP homopolymer, with high melt flow rate, high stiffness and low creep under load at elevated temperatures. This grade is delivered in 102297 color version. Applications: UnderhoodInformation provided by LyondellBasell. |