MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated lightly with oil typically used with machine parts. 3M™ Double Coated Tape 9496LE offers the added feature of 3M™ High Performance Acrylic Adhesive 200MP on one side to provide excellent bond strength to a variety of high surface energy substrates.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milFaceside Adhesive
 2.00 milCarrier
 2.00 milBackside Adhesive
 4.40 milCaliper
 6.70 milTotal Thickness
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 3.0625 pliStainless Steel, 90°, 15 min RT, Faceside; ASTM D3330
 3.6875 pliStainless Steel, 90°, 15 min RT, Backside; ASTM D3330
 4.75 pliStainless Steel, 90°, 72 hr RT, Backside; ASTM D3330
 5.5625 pliStainless Steel, 90°, 72 hr RT, Faceside; ASTM D3330
 6.9375 pliStainless Steel, 90°, 72 hr at 70°C, Faceside; ASTM D3330
 7.00 pliStainless Steel, 90°, 72 hr at 70°C, Backside; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °CLong term
 149 °CShort term
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
AppearanceBackside
 Faceside
LinerTan, 58# Polycoated Kraft
 Tan, 58# Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain CHR® 2302-3R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2253-2 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive
Permabond TA430 Acrylic Adhesive & Initiator

PMM33277 / 168024

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.