MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Asahi Kasei Leona™ 53G33 Polyamide 66, Heat Stabilized, GF Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Applications: Automotive parts, electrical & electronic parts, parts for office furnishings.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccDry as Molded; ASTM D792
Density 1.35 g/ccDry as Molded; ISO 1183
Moisture Absorption at Equilibrium 1.1 %
@Temperature 23.0 °C
50% RH; ISO 62
 1.1 %
@Temperature 23.0 °C
50% RH
Linear Mold Shrinkage, Flow >= 0.0030 cm/cmAsahi Kasei
Linear Mold Shrinkage, Transverse >= 0.0090 cm/cmAsahi Kasei
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88Conditioned at 50% RH; ISO 2039
 97Dry as Molded; ISO 2039
Hardness, Rockwell R 112Conditioned at 50% RH; ISO 2039
 121Dry as Molded; ISO 2039
Tensile Strength at Break 161 MPaConditioned at 50% RH; ISO 527
 203 MPaDry as Molded; ISO 527
Tensile Strength 170 MPaConditioned at 50% RH; ASTM D638
 215 MPaDry as Molded; ASTM D638
Elongation at Break 4.0 %Dry as Molded; ISO 527
 6.0 %Conditioned at 50% RH; ISO 527
Tensile Modulus 7.50 GPaDry as Molded; ISO 527
 9.50 GPaConditioned at 50% RH; ISO 527
Flexural Strength 250 MPaConditioned at 50% RH; ISO 178
 296 MPaDry as Molded; ISO 178
Flexural Modulus 7800 MPaConditioned at 50% RH; ISO 178
 9700 MPaDry as Molded; ISO 178
Izod Impact, Notched 135 J/mDry as Molded; ASTM D256
 158 J/mConditioned at 50% RH; ASTM D256
Charpy Impact Unnotched 92.0 kJ/m²Conditioned at 50% RH; ISO 179
 92.0 kJ/m²Dry as Molded; ISO 179
Charpy Impact, Notched 13.0 kJ/m²Dry as Molded; ISO 179
 15.0 kJ/m²Conditioned at 50% RH; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°CDry as Molded; ASTMD 696
Thermal Conductivity 0.400 W/m-KDry as Molded
Deflection Temperature at 1.8 MPa (264 psi) 208 °CDry as Molded; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Leona® 1300S Nylon 66
Asahi Kasei Leona™ 90G33 Polyamide 66, GF Reinforced
Envalior Akulon® N24-G6 PA6-GF30
H.C. Starck Amperit® 539.054 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt-Chromium (WC-WB-Co-Cr) 60-30-5-5
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets

PASAHI8140 / 221167

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.