Description: Thermoplastic elastomer SEBS (styrene ethylene butylene styrene) block copolymer 506 has high transparency, excellent processing performance, can be widely used in wire and pipe and other fields. Medical grade SEBS polymerYH-506 can replace the soft PVC manufacturing infusion tube, to avoid the damage to the human body by soft PVC in the processing of plasticizer do not meet the requirements of the FDA . Application: Compounding/Medical Formula: YH-506 67.5 SEBS polymer (YH-506): 67.5 Polypropylene: 30 Propylene wax: 2.5 Information provided by BEC Materials, LLC |