Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This product does not contain the flame retardants mentioned in the WEEE directive (PBB or PBDE). The product is used widely throughout the electrical and appliance industries for applications like pressure switches, circuit breaker housings, contactors, timers and programmers. Key characteristics: - UL listed V0 at 3.0 and 0.8 mm
- UL listed GWIT 825 °C and GWFI 960°C at 0.8 mm, compliant with IEC 60335-4
- UL listed on CTI PCL 1 (CTI = 425 V)
- Excellent mechanical performance
- Colorable in light colors
- Easy processing
Information provided by NILIT. |