MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 46/CF/15 Polyamide 46 with carbon fiber, heat stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: Properties/attributes include: Strong, stiff parts. Reduced moment of inertia compared with metal parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Gear parts for automotive appliances, control disks, cams, sliding elements.

Processing: During processing the moisture level should not exceed 0.1%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Excessively high predrying temperatures may cause discoloration. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccISO 1183
Moisture Absorption <= 1.00 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmDIN 16901
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 220 MPaISO 527-2
Elongation at Break 2.5 %ISO 527-2
Modulus of Elasticity 12.0 GPaISO 527-2
Flexural Strength 315 MPaISO 178
Flexural Modulus 10.0 GPaISO 178
Flexural Strain at Break 3.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1e+05IEC 60167
Surface Resistance <= 10000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°CDIN 53752
Thermal Conductivity 0.350 W/m-KDIN 52612
Maximum Service Temperature, Air 150 °CContinuous; UL 746B
 160 °CShort Term
Vicat Softening Point 290 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 330 °C
Zone 1 285 - 315 °C
Zone 2 305 - 315 °C
Zone 3 305 - 315 °C
Melt Temperature 310 °C
Mold Temperature 90.0 - 130 °C
Drying Temperature 80.0 °C
@Time 7200 - 28800 sec
Dehumidifying dryer
 80.0 °C
@Time 7200 - 43200 sec
Vacuum Dryer
Moisture Content <= 0.10 %
 
Descriptive Properties
Colornatural color (black)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast and Aged
Overview of materials for Nylon 6, 40% Glass Fiber Filled
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Nylon 6, 50% Glass Fiber Filled

PLUU8917 / 193876

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.