MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR V3900WX PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX V3900WX is an unreinforced, UV stabilized, weatherable, impact modified flame retardant Polybutylene Terephthalate/Polycarbonate (PBT) injection moldable grade. It has excellent chemical resistance and a UL94V0@1.5mm and 5VA@3.0mm flame rating. This is an excellent candidate for a wide variety of applications including outdoor enclosures requiring UL746C F1 weatherability performance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Density 1.30 g/ccISO 1183
Water Absorption 0.10 %23°C/sat; ISO 62
Moisture Absorption 0.0300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 11 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPa50 mm/min; ISO 527
 43.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPaSABIC - Japan Method
 51.0 MPa50 mm/min; ISO 527
 53.0 MPa50 mm/min; ASTM D638
Elongation at Break 42 %50 mm/min; ISO 527
 50 %50 mm/min; ASTM D638
 250 %SABIC - Japan Method
Elongation at Yield 4.0 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2090 MPa1mm/min; ISO 527
 2200 MPa5 mm/min; ASTM D638
Flexural Yield Strength 73.0 MPa2 mm/min; ISO 178
 80.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2130 MPa2 mm/min; ISO 178
 2200 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 800 J/mASTM D256
 110 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 45.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 52.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
 50.0 J
@Temperature -40.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 6.02e+16 ohmASTM D257
Dissipation Factor 0.0199
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 88.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 88.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 89.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 89.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 119 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 75.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 96.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 105 °CRate B/50; ASTM D1525
 121 °CRate B/50; ISO 306
 123 °CRate B/120; ISO 306
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 120 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 5VA
@Thickness 3.00 mm
UL 94
Glow Wire Test 725 °C
@Thickness 3.00 mm
IEC 60695-2-13
 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 260 °CInjection Molding
Zone 1 240 - 255 °C
Zone 2 245 - 260 °C
Zone 3 250 - 265 °C
Melt Temperature 250 - 265 °C
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 50 - 80 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10349 / 243816

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.