MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® HDC-G-327 - 3/16 - 15.0 (R2) Heavy Density Core  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Composite Fibers

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with either a thermoplastic or thermoset resin for the web impregnations. The product was developed for use in temperatures up to 500°F. Depending on the constituent resin system, the product may be suitable for short exposures at higher temperatures.

Features: High compression strength non-metallic honeycomb available; Formability tailored to customer's needs; Low-moisture pickup; High thermal stability, very low coefficient of thermal expansion; Proven history in service; High corrosion resistance.
Applications: HexWeb® HDC is used in sandwich structure as a replacement for potting compound in hard points or where extremely high compressive or shear strength is required. Using HexWeb® HDC in lieu of potting compound reduces process steps, improves part quality and reduces weight in the overall structure.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength 3.20 ksiStabilized
Shear Strength 1.20 ksiLong Beam Shear, W Direction
 1.80 ksiLong Beam Shear, L Direction

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core
Solvay CYCOM® 381 Epoxy Prepreg with IM7 Uni-graphite and 148FAW Epoxy
Hexcel® Fibrelam® 2000 Grade 1 Panels for Aircraft Flooring
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg

PHEXC386 / 98857

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.