MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® CleanGrip® 2103 Water based frictionizing agent
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: CleanGrip® is a sprayable water-based coating applied by bag manufacturers and corrugators to reduce the skid of paper packaging. Made of high-performance silica, it eliminates the build-up and clogging associated with alumina nonskids. CleanGrip ™ 2103 is designed to be applied by spray coater on the corrugator but may also be applied using felts, sponges or rollers. Usage: A high solids sprayable nonskid coating that provides excellent slide angles, is easily cleanable and hot melt and cold set gluable.

Applications (properties imparted): Industrial skid resistance.

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 8.5 - 9.5
Brookfield Viscosity <= 50 cPSpindle #1. 60 RPM.
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceThin, translucent liquid
Solids TypeSilica

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHE9904 / 287499

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.