MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Durethan® C 38 FKS 000000 Copolyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Copolyamide, film quality, high transparency, with processing aid, nucleated

Application Examples: blown film coextrusion (outer layer)

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Absorption 10 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 3.0 %23°C/50% R.H.; Test Sim. to ISO 62
Melt Flow 6 g/10 min
@Load 2.16 kg,
Temperature 235 °C
Estimated using room temperature density; ISO 1133
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Conditioned; IEC 60250
Dielectric Strength 30.0 kV/mmConditioned; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 212 °C10°C/min; ISO 11357-1/-3
 
Descriptive Properties
ISO Short NameISO 1874-PA 6/IPDI, FS,18-030N
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANX0796 / 99011

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.