Sandvik 15R10 is an austenitic chromium nickel (CrNi) stainless steel used as a base material for Sandvik coated strip steel. The product is particularly suited to many types of electric load carrying spring applications, such as contact springs and tactile domes. Sandvik 15R10 is characterized by good corrosion resistance, mechanical strength and excellent fatigue and relaxation properties, as well as superior contact properties and/or solderability, achieved through the right choice of coating layer.Information provided by Sandvik |