Made by microsuspension polymerization for plastisol preparation.
MAIN APPLICATIONS
Spread coating :
- artificial leather compact layer
- artificial leather foam layer.
Molding and dipping.
Spraying :
- Polyurethane sealants.
ADVANTAGES
- Good acceptance in Polyurethane formulations. Information provided by SolVin. SolVin is a predecessor company to Inovyn. |