MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gougeon Brothers PRO-SET® LAM-125/LAM-224 Laminating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Low viscosity for quick wet out of synthetic composite fabrics; especially effective with Kevlar® and carbon fiber.
Fast cure speed hardener provides 40 minute working time at 77°F (25°C). A typical laminate will be gelled in about 1.5 to 2 hours.
Optimized for hand wet out and machine impregnation in contact molding, vacuum bagging and Light RTM applications.
Room temperature cure properties suitable for many composite components and structures.
Tg as high as 193°F (90°C) with proper post cure providing excellent temperature stability and great part cosmetics.
Cost effective, high performance epoxy formulation for synthetic composite manufacturing.
Quality-control tinting is available at no extra charge; simply add "QC" after the product code on your order.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccHardener
 1.15 g/ccResin
 1.16 g/ccCured
Viscosity 75 cP
@Temperature 22.0 °C
hardener; ASTM D2196
 200 cP
@Temperature 48.9 °C
Mixed
 500 cP
@Temperature 29.4 °C
Mixed
 501 cP
@Temperature 29.0 °C
Mixed; ASTM D2196
 616 cP
@Temperature 25.0 °C
Mixed; ASTM D2196
 694 cP
@Temperature 22.0 °C
Mixed; ASTM D2196
 1100 cP
@Temperature 15.6 °C
Mixed
 1731 cP
@Temperature 22.0 °C
resin; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D2240
 82
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D2240
 85
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D2240
 86
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D2240
 87
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D2240
Tensile Strength 10900 psi
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D638
 11000 psi
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 11000 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 11100 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 11400 psi
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D638
Elongation at Break 3.2 %
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D638
 4.0 %
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D638
 5.6 %
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 5.6 %
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 5.6 %
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
Tensile Modulus 495000 psiRT Gelation; ASTM D638
 522000 psiRT Gelation; ASTM D638
 535000 psiASTM D638
 547000 psiRT Gelation; ASTM D638
 572000 psiASTM D638
Flexural Strength 17500 psi
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D790
 18300 psi
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D790
 18900 psi
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 18900 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 19700 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
Flexural Modulus 475000 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 507000 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 512000 psi
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 526000 psi
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D790
 541000 psi
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D790
Compressive Yield Strength 14600 psi
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D695
 14600 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D695
 14600 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D695
 15800 psi
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D695
 16300 psi
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D695
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °F
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
ASTM D648
 137 °F
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
ASTM D648
 148 °F
@Treatment Temp. 49.0 °C,
Time 28800 sec
RT Gelation; ASTM D648
 161 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D648
 179 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D648
Glass Transition Temp, Tg 193 °FASTM E1356
 138 °F
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
DSC Onset– 1st Heat, 1 Hz, 3°C per minute; ASTM E1356
 139 °F
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
DSC Onset– 1st Heat, 1 Hz, 3°C per minute; ASTM E1356
 151 °F
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
DMA Onset Storage Modulus, 1 Hz, 3°C per minute; ASTM E1640
 151 °F
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
DMA Onset Storage Modulus, 1 Hz, 3°C per minute; ASTM E1640
 155 °F
@Treatment Temp. 49.0 °C,
Time 28800 sec
DSC Onset– 1st Heat, RT Gelation, 1 Hz, 3°C per minute; ASTM E1356
 170 °F
@Treatment Temp. 22.0 °C,
Time 2.42e+6 sec
DMA Peak Tan Delta, 1 Hz, 3°C per minute; ASTM E1640
 170 °F
@Treatment Temp. 25.0 °C,
Time 1.21e+6 sec
DMA Peak Tan Delta, 1 Hz, 3°C per minute; ASTM E1640
 171 °F
@Treatment Temp. 49.0 °C,
Time 28800 sec
DMA Onset Storage Modulus, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 177 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
DMA Onset Storage Modulus, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 178 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
DSC Onset– 1st Heat, RT Gelation, 1 Hz, 3°C per minute; ASTM E1356
 184 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
DSC Onset– 1st Heat, RT Gelation, 1 Hz, 3°C per minute; ASTM E1356
 193 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
DMA Onset Storage Modulus, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 195 °F
@Treatment Temp. 49.0 °C,
Time 28800 sec
DMA Peak Tan Delta, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 201 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
DMA Peak Tan Delta, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 216 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
DMA Peak Tan Delta, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 
Processing PropertiesOriginal ValueComments
Cure Time 1.50 - 2.00 hourtypical laminate will be gelled
Pot Life 9.00 - 13.0 min
@Temperature 29.0 °C
150 g; ASTM D2471
 9.00 - 13.0 min
@Temperature 29.0 °C
500 g; ASTM D2471
 10.0 - 13.0 min
@Temperature 25.0 °C
500 g; ASTM D2471
 11.0 - 15.0 min
@Temperature 25.0 °C
150 g; ASTM D2471
 15.0 - 19.0 min
@Temperature 22.0 °C
150 g; ASTM D2471
 15.0 - 19.0 min
@Temperature 22.0 °C
500 g; ASTM D2471
Working Life 40.0 min
Shelf Life 24.0 Monthhardener
 36.0 Monthresin
 
Descriptive Properties
Mix ratio100:25.2–100:30.8Weight Range, Resin: Hardener
 100:28.6Weight, Resin: Hardener
 100:28.9–100:35.3Volume Range, Resin: Hardener
 100:33.3Volume, Resin: Hardener
 3.00:1Volume, Resin: Hardener
 3.47:1–2.84:1Volume Range, Resin: Hardener
 3.5:1Weight, Resin: Hardener
 3.96:1–3.24:1Weight Range, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGP908 / 290752

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.