MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott D 263® T eco Thin Borosilicate Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm to 1.1 mm. D 263® T eco borosilicate glass is available in standard stock size sheets or can be custom cut into round or square shapes. D 263® T eco thin glass is used as a substrate glass for coatings or replacement for plastic for applications in the automotive and electronics industries D 263® T eco is manufactured without adding arsenic and antimony as refining agents. It has been used in touch panel displays, optocaps for diode lasers, and other optical applications.

Information provided by SCHOTT North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.51 g/cc
Thickness 30.0 - 1100 micronswide range available
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.7
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 µm/m-°C
@Temperature 20.0 - 300 °C
Transformation Temperature, Tg 557 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.523
@Wavelength 588 nm
nd
Transmission, Visible 91.7 %
@Thickness 1.1 mm
TvD65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borosilicate Glass
Schott D 263 Thin Borosilicate Glass
Borosilicate Glass, Low Expansion
Corning Borosilicate Specialty Glass Pressed Parts
Fused Quartz

CSGS130 / 138090

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.