MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess Uniplex 165 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 165 is an effective plasticizer for imparting low temperature flexibility to various polymers. It is compatible with cellulose esters, polyvinyl acetate (PVAc), polyvinyl chloride (PVC), vinyl chloride vinyl acetate copolymers (VCVAC) and rubber. Uniplex 165 is suggested as a solvent respectively plasticizer in fingernail enamel, nail enamel remover, hair sprays, adhesives, and coatings.

Chemical composition: Di-isobutyl adipate (DiBA)

General Uniplex 165 is an effective plasticizer for imparting low temperature flexibility to various polymers. Uniplex 165 is suggested as a solvent respectively plasticizer in cosmetics, adhesives, and coatings. It is compatible with cellulose esters inclusive cellulose acetate butyrate (CAB) and cellulose nitrate (CN), polyvinyl acetate (PVAc), polyvinyl chloride (PVC), vinyl chloride vinyl acetate copolymers (VCVAC), and rubber (CR, EVA).

Applications: Uniplex 165 is characterized by a good compatibility with a large number of polymers. It is an effective plasticizer for imparting low temperature flexibility, with a good balance of solvation and low temperature properties. Uniplex 165 is suggested as a solvent respectively plasticizer in fingernail enamel, nail enamel remover, hair sprays, adhesives, and coatings. Uniplex 165 has a very low viscosity and a high volatility. Uniplex 165 is used when US regulations and recommendations governing food contacting applications need to be met. More information is available on request.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/cc
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.43
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %Karl Fischer
Shelf Life 12.0 Month
 
Descriptive Properties
Appearanceclear liquid
Color<25Hazen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9101 / 209492

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.