MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ FE 5660Q Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Fluoroelastomer FE 5660Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, FE 5660Q should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks display excellent processing characteristics and storage stability.
  • Composition: Di-polymer of vinylidene fluoride and hexafluoropropylene
  • High viscosity version of FE 5620Q and FE 5640Q
  • Process targets: compression molding
  • Improved scorch resistance at high molding temperatures
  • Proprietary incorporated cure technology
  • Excellent mold release
  • Improved cure technology resulting in more consistent part size from successive molding cycles
  • Clean running

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Mooney Viscosity 60
@Temperature 121 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 2400 psiPress Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 200 %Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 1.15 ksi
@Strain 100 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 9.0 %
@Temperature 200 °C,
Time 252000 sec
O-rings -214; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature -18.0 °CTR10; ASTM D1329
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 65.9 %
 
Descriptive Properties
ColorOpaque Off-White
MH, Maximum Torque24.4 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
 25.3 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque2.3 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
 2.3 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
SolubilityKetones and Esters
t`50, Time to 50% cure0.7 minutes100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
 2.6 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t`90 - Time to 90% cure0.8 minutes100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
t`90 - Time to 90% cure 3.5 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ts2 - Time to 2 in-lb rise from min 0.6 minutes100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
 2 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDYNE132 / 34940

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.