MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP121CL-LO Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, High Temperature

Material Notes: Key Features:
  • Low viscosity
  • Electrically insulative
  • Very long open time
  • Excellent temperature resistance and physical strength
  • Impressive optical clarity
  • Meets NASA low outgassing specifications
Product Description: Master Bond EP121CL-LO is a two component, high performance epoxy resin system that features very low viscosity and an extraordinary long open time at room temperature of at least 2-3 days. It does, however, require oven curing. The mix ratio is a relatively easy to use 100:80, by weight. A typical cure schedule is 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F, although, a number of variations are possible. It has excellent adhesion to a wide variety of substrates including metals, composites, glass, ceramics and many rubbers and plastics. EP121CL-LO is particularly prominent for applications involving rigorous electrical insulation properties. Another attractive feature is its excellent physical strength profile. It offers superior chemical resistance to water, oils, acids, bases, fuels and many solvents. The service temperature range is -80°F to +500°F. EP121CL-LO is a specialty type system that issued in a variety of aerospace, electronic and OEM type applications.

Product Advantages:

  • Low viscosity
  • Extraordinarily long open time
  • Splendid thermal stability
  • Marvelous electrical insulation properties
  • First rate physical properties
  • Great optical clarity
  • Meets NASA low outgassing

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 150 - 300 cPPart B
 1000 - 3000 cPmixed
 10000 - 14000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80
Tensile Strength >= 12000 psi
Tensile Modulus >= 450000 psi
Compressive Strength >= 15000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 3.60e+11 ohm-cm
@Temperature 150 °C
 >= 3.00e+12 ohm-cm
@Temperature 100 °C
 >= 3.00e+14 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 3.01
@Frequency 1e+6 Hz,
Temperature 25.0 °C
 3.25
@Frequency 60 Hz,
Temperature 25.0 °C
 3.28
@Frequency 1000 Hz,
Temperature 25.0 °C
 3.38
@Frequency 60 Hz,
Temperature 100 °C
 3.41
@Frequency 1000 Hz,
Temperature 100 °C
 3.74
@Frequency 60 Hz,
Temperature 150 °C
 3.87
@Frequency 1000 Hz,
Temperature 150 °C
Dissipation Factor 0.010
@Frequency 1e+6 Hz,
Temperature 100 °C
 0.012
@Frequency 1e+6 Hz,
Temperature 150 °C
 0.020
@Frequency 1e+6 Hz,
Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 45.0 µm/m-°C
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -80.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.56
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 121 °C
followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F
Working Life 1440 - 4320 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio100:80 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM912 / 185505

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.