MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Manufacturing Insight EFR-1FM Enhanced Fire Retardant Additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: EFR-1FM is ideal for incorporation into reinforced (carbon fiber, Kevlar fiber, glass fiber) thermoset resin systems, including coatings and foams, potting compounds, fiberglass reinforced structures as well as electronic laminates and other similar applications. EFR-1FM has been proven especially successful in epoxy resin systems, but also functions well in acrylic, vinyl acetate, urethane and PVC resin systems.

When blended into a resin system, EFR-1FM will react to heat and/or flame by foaming and forming a thick, high yield char barrier. The char barrier will extinguish fire and prevent further flame spread. Additionally, the char foam insulates and protects the coated substrate from heat and fire damage.

EFR-1FM is halogen-free, contains no PBDEs, PBBs or other brominated compounds and does not evolve the highly toxic and corrosive gasses associated with many other fire retardants. EFR-1FM enhanced fire retardant additive is a RoHS/WEEE compliant material. EFR-1FM functions at loading levels in the range of 10%-20% by weight. Flame spread and smoke developed values (ASTM E-84) are typically 10/10 and under and are in compliance with UL 94VO, IMO MSC.41(64) and FAR 25.853

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solubility in Water <= 1.0 %At 170°F
Particle Size 3.0 - 5.0 µm
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
 
Descriptive Properties
AppearanceVery fine free flowing white powder
Char Activation Temp300°C
Char Forming Efficiency99% Minimum
Purity98% Minimum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® Mat VMA Carbon Fiber
Solvay Thornel® Graphite Cloth
Solvay CYCOM® 2237 Polyimide Resin System
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing

PMFGINS1 / 52929

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.