MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.77 - 1.80 g/ccASTM D792
Water Absorption 0.030 - 0.050 %ASTM D570
Viscosity 400000 - 800000 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Melt Flow 4.0 - 25 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 15 g/10 min
@Load 3.80 kg,
Temperature 232 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 75ASTM D2240
Tensile Strength at Break 27.6 - 48.3 MPaASTM D638
Tensile Strength, Yield 31.0 - 41.4 MPaASTM D638
 40.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 30 - 200 %ASTM D638
Elongation at Yield 5.0 - 15 %ASTM D638
 10 %Dry; ISO 527-1/-2
Tensile Modulus 1030 - 1520 MPaASTM D638
 1300 MPaDry; ISO 527-1/-2
Flexural Strength 20.7 - 34.5 MPa
@Strain 5.0 %
ASTM D790
Flexural Modulus 1030 - 1240 MPaASTM D790
Compressive Strength 41.4 - 58.6 MPaASTM D695
Izod Impact, Notched 107 - 427 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Charpy Impact, Notched 8.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
Coefficient of Friction, Dynamic 0.19vs. steel; ASTM D1894
Coefficient of Friction, Static 0.26vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 6.0 - 9.0CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm65% R.H; ASTM D257
Dielectric Constant 3.5 - 10.2
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.30 - 1.60 kV/mmASTM D149
Dissipation Factor 0.010 - 0.22
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 126 - 185 µm/m-°CASTM D696
Specific Heat Capacity 0.745 - 0.958 J/g-°CDSC
Thermal Conductivity 0.144 - 0.180 W/m-KASTM D433
Melting Point 157 °C10°C/min; Dry; ISO 11357-1/-3
 155 - 160 °CASTM D3418
Maximum Service Temperature, Air 140 °CUL RTI
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 75.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CDry; ISO 75-1/-2
 37.8 - 55.0 °CASTM D648
Glass Transition Temp, Tg -40.0 °C10°C/min; Dry; ISO 11357-1/-2
 -40.6 - -38.3 °CASTM D7028
Decomposition Temperature 375 °C1% wt. loss, TGA, in air
 410 °C1% wt. loss, TGA, in nitrogen
UL RTI, Electrical 140 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
Yellow Card Available; Dry; IEC 60695-11-10
Oxygen Index 43 %ASTM D2863
 43 %Dry; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.42sodium D line; ASTM D542
 
Descriptive Properties
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Goodfellow Aluminum 99/Silicon 1 Alloy
Arkema KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PARKG920 / 144545

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.