MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Polene PE100N Polypropylene Wax
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.930 g/ccTPI Method
Viscosity 1.0 - 30 cPASTM D445
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 5.0 - 25
@Temperature 25.0 °C
ASTM D1321
 
Thermal PropertiesOriginal ValueComments
Melting Point 108 - 124 °CASTM D127
 
Descriptive Properties
ColorPale-White
Product FormFlake

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade
Hyosung Topilene C500H PP
BASF Novolen® 3520 L Polypropylene

PIRPC041 / 84018

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.