MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Dynasol Solprene® 233 Medium CIS Polybutadiene
Categories: Polymer; Thermoset

Material Notes: Solprene 233 is a medium cis polybutadiene used in applications where good performance at low temperatures and excellent abrasion resistance are needed. It is designed for critical processing applications with enhanced mixing and processability. It is packaged in bales wrapped with low melting point polyethylene film.

Information provided by Dynasol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccDIN 53479
Mooney Viscosity 35
@Temperature 100 °C
ML 1+4; ASTM D1646
 <= 75
@Temperature 100 °C
Compounded, ML 1+4; ASTM D1646
Ash <= 0.25 %ASTM D1416
Collected Volatile Condensable Material <= 1.0 %ASTM D1416
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 11.0 MPaCompounded, 35 mins.; ASTM D3185
Elongation at Break >= 360 %Compounded; ASTM D3185
300% Modulus 0.00800 GPa
@Strain 300 %
Compounded, 35 mins.; ASTM D3185
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -92.0 °CNM 300-58
 
Descriptive Properties
Antioxidant Content0.2 %NM 300-52
ColorMax 3NM 300-39
Free SoapMax 0.03 %ASTM D1416
Organic AcidMax 0.03 %ASTM D1416

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical BR 1208 Polybutadiene Polymer
Polybutadiene Rubber (BR)
DuPont Mobility and Materials Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
Dynasol Solprene® 200 Polybutadiene Rubber
Dynasol Solprene® 200P Polybutadiene Rubber

PDYNA04 / 34752

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.