Europrene Latice® 5585 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant. Key Features: Europrene Latice® 5585 shows excellent performances at high filler loading. Main Applications: Europrene Latice® 5585 is used for primary and secondary backings when a soft handle is required. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |