MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
RAUH Polymers Optimum® 800 Metal Flake COPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Optimum® copolyesters are a new development in polymer technology. They can meet the requirements and desires of engineers for the most demanding applications and cost effectiveness to enable the broadest possible applications. Optimum is a hard block copolyester of either, or both, crystalline and amorphous blocks, depending on grade. The Optimum use is for applications that require high scratch and mar resistance, heat, UV and chemical resistance. The appearance of Optimum can be optically clear. Optimum in colors and tints can accept fillers such as metal flake without the loss of properties. The processability is superior, and the cost saving is tremendous with the elimination of painting parts. As with other engineering thermoplastics, Optimum resin can be injection molded using standard equipment. The characteristic rheological behavior makes it easy to process, with good fill over long flow lengths at low pressure, with faster cycle times. Optimum grades cal also be extruded, blow molded or thermoformed.

Basic Properties: Optimum® copolyesters are a class of engineering polymers offering unmatched properties in combinations of high level mechanical, thermal, chemical and electrical properties:

  • High tensile and elongation
  • Abrasion, scratch and mar resistant
  • No break notched izod
  • High modulus
  • Ductile - can accept multiple bends and impacts without cracking or failure
  • No stress whitening
  • Hard with dart impact of >320 IP
  • HDT of >125 degrees C
  • Stability
  • Impact resistant
  • UV stable <3 DE color change 3000 kg
  • Excellent chemical resistance
  • Heat resistance >1000 hrs @ 150 degrees C
  • Ozone, water and hydrolysis
  • Cold resistance <-40 degrees C
  • Dishwasher safe

Information provided by Rauh Polymers Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0127 - 0.0203 cm/cmType 1 Bar
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 in/inASTM D955
Melt Flow 50 g/10 min
@Load 1.20 kg,
Temperature 300 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 7000 psiType 1 Bar; ASTM D638
Elongation at Break 120 %Type 1 Bar; ASTM D638
Flexural Modulus 300000 psiASTM D790
Izod Impact, Notched 12.0 ft-lb/inASTM D256
Dart Drop, Total Energy >= 320 ft-lb
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAUH005 / 296465

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.