Multranol 9158 is a propylene oxide-based triol. Properties / Applications: Multranol 9158 is a propylene oxide-based triol. It has good compatibility with foam ingredients and is useful for reduced system viscosity. It is used as a copolyol for a variety of low- and high-density polyurethane formulations. These include insulated panels, thermal break and decorative molding. As with any product, use of Multranol 9158 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |