INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form. INNOPOL® CS 3-8000 FR is highly suitable for manufacturing indoor waste water discharge system parts. This grade is a flame-retarded material, where the classification of flame retardancy is B2 according to DIN 4102. Information provided by INNO-COMP |