MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene NA490177 Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Petrothene NA490177 is a LDPE/EVA copolymer resin selected for use in specialty films. NA490177 contains antiblock and is used to produce film with excellent puncture resistance, impact strength, heat sealability, clarity and low temperature flexibility. Typical applications include frozen food packaging, bundling and heavy-duty bags. Applications: Agriculture Film, Bags & Pouches, Film Wrap, Food Packaging Film, Heavy Duty Packaging, Liner Film, Sealants, Shrink Film, Stretch Hood

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.923 g/ccASTM D1505
Density 0.926 g/ccASTM D1505
Vinyl Acetate Content 4.5 %LYB Method
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 6000 ppmLYB Method
Slip Level 0.000 ppmLYB Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 370 %ASTM D882
Film Elongation at Break, TD 550 %ASTM D882
Elmendorf Tear Strength MD 150 gASTM D1922
Elmendorf Tear Strength TD 250 gASTM D1922
Dart Drop Test 320 gF50; ASTM D1709
Film Tensile Strength at Break, MD 22.1 MPaASTM D882
Film Tensile Strength at Break, TD 20.7 MPaASTM D882
1% Secant Modulus, MD 131 MPaASTM D882
1% Secant Modulus, TD 159 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 88.0 °CASTM D1525
 
Descriptive Properties
Processing MethodBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT8865 / 220499

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.