MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials BETAMATE™ 1060N US epoxy resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: One component, epoxy based adhesive especially developed for the body shop.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 845
Solids Content >= 99 %
Viscosity >= 7500 cP
@Temperature >=50.0 °C
Casson; D(1s) 1.075
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 1798
Tensile Modulus 2900 MPaISO 527-1/-2
Adhesive Bond Strength >= 26.0 MPaLap shear strength after 3 days; DIN EN 1465
Peel Strength 9.00 kN/mT-Peel; ISO 11339
 23.0 kN/mImpact-Peel; ISO 11343
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 110 °CFreezing; 10°C/min; ISO 11357-1/-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 30.0 - 65.0 °C
Cure Time 0.500 hour
@Temperature 180 °C
Shelf Life 9.00 Month
@Temperature 5.00 - 25.0 °C
 
Descriptive Properties
Basisepoxy resin
ColorBlue
CompatibilityMetals
PolymerAdhesive
Regional AvailabilityNorth America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4501 / 280447

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.