MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Pressure Seal 23511 Ethylene Propylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 23511 is a 50 durometer black colored general purpose EPDM elastomer. It exhibits good resistance to heat, compression set and water. It will remain non brittle at low temperatures. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 AA 512 A13 F17 C12 EA14; 3 AA 512 B13 B33 EA14 F17 G21; 2 BA 510 C12 F17; 8 BA 510 B13 C12; 3 CA 510 A25 B44 B35 C32 EA14 F17 F18 G21; 2 DA 510 A26 B36 C32 EA14 F19 G21

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 54
 54
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 54
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 56
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 57
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 57
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 58
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 58
@Temperature 150 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1507 psi
 1481.4 psi
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 1567.3 psi
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 1588.4 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 1588.4 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1793.3 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1793.3 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 474 %
 412.9 %
@Temperature 70.0 °C,
Time 252000 sec
Heat Aged
 479.2 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 479.2 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 503.9 %
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 534.2 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 534.2 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
100% Modulus 175 psi
Tear Strength 96.0 pliDie B
 150 pliDie C
Compression Set 12.5 %
@Temperature 100 °C,
Time 79200 sec
Plied
 13.5 %
@Temperature 100 °C,
Time 79200 sec
Solid
 14.6 %
@Temperature 125 °C,
Time 79200 sec
Plied
 15.2 %
@Temperature 100 °C,
Time 252000 sec
Solid
 17.3 %
@Temperature 100 °C,
Time 252000 sec
Plied
 17.6 %
@Temperature 150 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -105 °F
Shrinkage 1.5 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL219 / 318429

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.