MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40), M07 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Continuous Cast

Casting Characteristics: High – Casting Yield, Effect of Section Size; Medium – Fluidity, Gassing, Shrinkage in Solidification, Shrinkage During Freezing; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Coated Metal Arc Welding

Typical uses: Ornamental Fixtures; Hardware; Cooling Equipment; Lightning Protection; Trowels for Cement Working; Electrical Equipment; Electrical Hardware; Switches; Large Hold Down Screws; Air Actuators; Bearing Segments for Steel Industry; Bearings; Bushings; Couplings; Furnaces; Handles for Dental Equipment; Impellers; Low Pressure Valves; Pressure Blocks for Steel Industry; Printing Presses; Pump Fixtures; Pump Parts; Pumps; Rings; Small Gears; Transducer Housings; Valve Bodies; Valve Bodies for the Water Meter Industry; Valves; Valves for the Water Meter Industry; Marine Products; Parts for Boats; Faucets; Fixtures; Pipe Fittings

Applicable Specifications: As Centrifugal Cast – Castings AMS 4855, Castings SAE J462, Castings SAE J461, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings ASTM B62, Castings SAE J462, Castings ASTM B584, Castings ASME SB62, Castings AMS 4855, Castings SAE J461; Fitting – ASTM B62, ASME SB62, ASME B16.32, FEDERAL WW-P-460, ASME B16.23, ASME B16.26, ASME B16.18, ASME B16.15; Flanges – ASTM B62, ASME SB62, ASME B16.24; Ingot - ASTM B30; Precision Cast – Castings MILITARY MIL-C-11866; Unions – FEDERAL WW-U-516; Valves – MILITARY MIL-V-18436

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.318 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 30.0 ksi
Tensile Strength, Yield >= 19.0 ksi0.5% Ext
Elongation at Break >= 19 %
Tensile Modulus 13500 ksi
Machinability 84 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000115 ohm-cm15% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 41.6 BTU-in/hr-ft²-°F
Melting Point 1570 - 1850 °F
Solidus 1570 °F
Liquidus 1850 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.25 %
Copper, Cu 84 - 86 %
Iron, Fe <= 0.30 %
Lead, Pb 4.0 - 6.0 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.080 %
Tin, Sn 4.0 - 6.0 %
Zinc, Zn 4.0 - 6.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC83600x2 / 293143

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.