MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo Celanex® 2002-9 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Product Description: Medium viscosity grade for short cycle times. Chemical abbreviation according to ISO 1043-1: PBT Molding compound ISO 7792-PBT, MGHR, 10-030 Polybutylenterephthalat, nucleated grade with high molecular weight.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Additive: Mold Release

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Melt Density 1.11 g/ccFill Analysis, Melt
Water Absorption 0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.45 %ISO 62
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cmISO 294-4
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8410 psiISO 527-2/50
Elongation at Break >= 50 %Nominal; ISO 527-2/50
Elongation at Yield 4.0 %ISO 527-2/50
Tensile Modulus 377000 psiISO 527-1
Charpy Impact Unnotched 90.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 2.60 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 2.90 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 580 V/milIEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.0 µin/in-°FISO 11359-2
Specific Heat Capacity 0.471 BTU/lb-°FFill Analysis, Melt
Thermal Conductivity 0.910 BTU-in/hr-ft²-°FFill Analysis, Melt
Melting Point 437 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 302 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 131 °FUnannealed; ISO 75-2/A
Vicat Softening Point 374 °FISO 306/B50
Flammability, UL94 HB
@Thickness 1.27 mm
 HB
@Thickness 1.52 mm
Oxygen Index 22 %ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 482 - 500 °FHot Runner
Feed Temperature 446 - 464 °FInjection
Rear Barrel Temperature 446 - 464 °F
Middle Barrel Temperature 455 - 482 °F
Front Barrel Temperature 455 - 482 °F
Nozzle Temperature 454 - 500 °F
Zone 4 464 - 500 °FInjection
Melt Temperature 455 - 500 °F
Mold Temperature 149 - 205 °F
Ejection Temperature 426 °FFill Analysis
Drying Temperature 248 - 266 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6164 / 310857

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.