Total Petrochemicals Polystyrene 850S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding. Suitable Applications for Total Petrochemicals Polystyrene 850S include TV covers, Decoders, Hi-Fi and Internal parts for office equipment. Information provided by Total Petrochemicals. |