MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BEWiSynbra Circulum® K-910e/p Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: K-910e and K-910p are expandable polystyrene grades containing pentane as a blowing agent. The products are delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3. K-910e is available in 1050 kg octabins and K-910p in 1100 kg octabins.

Applications: The properties of K-910e/p make it suitable for the production of thin-walled shape-moulded products as well as heavy insulation board by block moulding.

Information provided by BEWi Synbra

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Storage Temperature 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 0.240 MPa20 kg/m3; EN 12089
 0.380 MPa30 kg/m3; EN 12089
 0.560 MPa40 kg/m3; EN 12089
Compressive Strength 0.115 MPa
@Strain 10 %
20 kg/m3; EN 826
 0.200 MPa
@Strain 10 %
30 kg/m3; EN 826
 0.280 MPa
@Strain 10 %
40 kg/m3; EN 826
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0320 W/m-K30 kg/m3; EN 12667
 0.0320 W/m-K40 kg/m3; EN 12667
 0.0340 W/m-K20 kg/m3; EN 12667
 
Descriptive Properties
Raw material<0.1%Monomer level
 0.4-0.7 mmMain bead size distribution
 5.5-6.5%Pentane content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBEWS011 / 250820

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.