MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kohesi Bond KB 1427 HT-3 One component, rapid curing epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Superb electrical insulation
  • Snap curing
  • Impressive chemical resistance
  • Castable up to 1/4 inch thicknesses
  • Glass transition temperature (Tg) of 120°C
  • Unlimited working life at room temperature
Kohesi Bond KB 1427 HT-3 is an exclusive one component epoxy system that can cure completely in 2 - 3 minutes at 150°C. Although it requires a minimum temperature of 120°C for curing, it cures equally fast (3 - 5 minutes) at that temperature. KB 1427 HT-3 offers an extremely wide service temperature range of -50°C to +200°C, with an impressive glass transition temperature (Tg) of 120°C. This product’s unlikely low exotherm makes it ideal for use in potting up to 1/4 inch thicknesses. Being a one component system, it requires no mixing and provides ease of application. This epoxy system will not set-up unless heated above 100°C. KB 1427 HT-3 also adheres well to a wide variety of substrates including metals, ceramics, composites, most plastics and glass. It provides outstanding mechanical strength properties and dimensional stability. In addition to superior electrical insulation, KB 1427 HT-3 also offers first-rate chemical resistance. It has a yellow - brown color. This product is available in a paste version as well as in a toughened version for enhanced resistance to mechanical shock and thermal cycling. Owing to its splendid performance and ease of use, KB 1427 HT-3 is ideal for use in aerospace, electronics, chemical processing and various OEM applications.

Typical Applications:

  • Bonding
  • Sealing
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 80000 - 135000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 85
Tensile Strength 8500 psi
Adhesive Bond Strength >= 2200 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.81
@Frequency 60 Hz
Dielectric Strength >= 420 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 - 50.0 µm/m-°C
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg 120 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 min
@Temperature 150 °C
Option 2
 3.00 - 5.00 min
@Temperature 120 °C
Option 1
Shelf Life 6.00 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOHESI940 / 249119

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.