MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dioshy E963D-GS Thermoplastic Polyester Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Thermoplastic polyester elastomer (TPEE), high performance engineering elastomers; hardness range Shore D 30 ~ Shore D 72.

Features:

  • Excellent anti-fatigue and tough; suitable to engineering mechanical products.
  • Very good oil resistance and chemical resistance; good compression set; white color.
  • Good processing ability, suitable to mostly thermoplastic procedures.
  • Green material, passed heavy metal regulation, RoHS and EACH –SVHC .

      Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.233 g/ccJIS-K6301
Melt Flow 37.98 g/10 min
@Load 2.16 kg,
Temperature 230 °C
JIS-K7210
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63JIS-K6301
Tensile Strength 320 kg(f)/cm²JIS-K6310
Elongation at Break 541 %JIS-K6310
100% Modulus 197 kg(f)/cm²JIS-K6310
300% Modulus 65.0 kg(f)/cm²JIS-K6310
Tear Strength 2577 kg(f)/cmJIS-K6310-B
Compression Set 21 %
@Temperature 23.0 °C,
Time 79200 sec
JIS-K6301
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Strength 26.0 kV/mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 200 °CExtrusion
 195 - 205 °CInjection
Middle Barrel Temperature 200 - 210 °CExtrusion
 205 - 215 °CInjection
Front Barrel Temperature 200 - 210 °CExtrusion
 205 - 215 °CInjection
Nozzle Temperature 225 - 235 °CInjection
Die Temperature 215 - 225 °CExtrusion
Drying Temperature 100 °C
Dry Time 2.00 hour
 
Descriptive Properties
ColorWhite
TPEE TypeTPC-ET

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDIOSH047 / 294657

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.