Fine particle size. 33% bound ACN. Crosslinked polymer structure. CaCO3 partitioning agent. Can be used in TPU and phenolic blends. Used in friction materials such as disc-pads and brake linings. Omnova Solutions acquired this product line with the Eliokem acquisition. |