MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® LV-23H Nylon 12, 23% Glass Fiber Filled, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Glass Fiber, 23% Filler by Weight

Additive: Heat Stabilizer

Features: Heat Stabilizer; Hydrolysis Resistant

Uses: Appliance Components; Automotive Applications; Connectors; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Household Goods; Hydraulic Applications; Industrial Applications; Medical Devices; Pneumatic Applications; Power/Other Tools; Sporting Goods

RoSH Compliance: RoSH Compliant

Automotive Specifications: ASTM D4000 PA420 G23 A21640; ASTM D4000 PA420 G23 A91340 KB060 Color: L94302.05 Green; ASTM D4000 PA420 G23 A99690 AA002 CA170 CA116 JR110 KB090 MA115 UA034 YD160 Color: 9203 Black; CHRYSLERY MS-DB-41 CPN3363 Color: 9203 Black; CHRYSLERY MS-DB-41 CPN4568 Color: Natural; GM GMW15702-012391 PA12-GF23 Color: 9213 Black

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Water Absorption 0.60 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 1.2 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16000 psiISO 527-2
Elongation at Break 7.0 %ISO 527-2
Tensile Modulus 841000 psiISO 527-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 11.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 83.0 µin/in-°FISO 11359-2
Melting Point 352 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 248 °FLong Term; ISO 2578
 302 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 311 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 176 °FUnannealed; ISO 75-2/C
Minimum Service Temperature, Air 194 °FLong Term; ISO 2578
Flammability, UL94 HB
@Thickness 0.762 mm
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGRIM160 / 307519

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.